Brand |
Chemical Analysis(%) |
Physical Property |
SiO2 |
Al2O3 |
Fe2O3 |
CaO |
MgO |
Cr2O3 |
C.C.S(Mpa) |
A.P.(%) |
B.D.(g/cm3) |
Refractoriness under load (℃) |
20 |
1.2 |
8.0 |
9.0 |
1.5 |
60 |
20 |
50 |
16 |
3.20 |
1700 |
18 |
1.2 |
8.0 |
8.0 |
1.5 |
62 |
18 |
50 |
16 |
3.20 |
1700 |
16 |
1.5 |
7.0 |
8.0 |
1.5 |
65 |
16 |
50 |
16 |
3.18 |
1700 |
14 |
1.5 |
6.0 |
7.0 |
1.5 |
67 |
14 |
45 |
16 |
3.18 |
1700 |
Description
High strength, corrosion resistance, erosion resistance, good slag resistance and thermal shock stability.
Application
nonferrous furnace, steel making EAF, converter, AOD, VOD, and refining ladle. |